非高纯氧化钪制备高纯无水氯化钪熔盐的试验

肖军辉, 梁冠杰, 黄雯孝, 丁威, 彭杨, 吴强. 非高纯氧化钪制备高纯无水氯化钪熔盐的试验[J]. 矿产综合利用, 2018, (6): 57-61,47. doi: 10.3969/j.issn.1000-6532.2018.06.011
引用本文: 肖军辉, 梁冠杰, 黄雯孝, 丁威, 彭杨, 吴强. 非高纯氧化钪制备高纯无水氯化钪熔盐的试验[J]. 矿产综合利用, 2018, (6): 57-61,47. doi: 10.3969/j.issn.1000-6532.2018.06.011
Xiao Junhui, Liang Guanjie, Huang Wenxiao, Ding Wei, Peng Yang, Wu Qiang. Test of Using Non Highly Purified Scandia Preparation of Highly Purified Anhydrous Scandium Trichloride Fused Salt[J]. Multipurpose Utilization of Mineral Resources, 2018, (6): 57-61,47. doi: 10.3969/j.issn.1000-6532.2018.06.011
Citation: Xiao Junhui, Liang Guanjie, Huang Wenxiao, Ding Wei, Peng Yang, Wu Qiang. Test of Using Non Highly Purified Scandia Preparation of Highly Purified Anhydrous Scandium Trichloride Fused Salt[J]. Multipurpose Utilization of Mineral Resources, 2018, (6): 57-61,47. doi: 10.3969/j.issn.1000-6532.2018.06.011

非高纯氧化钪制备高纯无水氯化钪熔盐的试验

  • 基金项目:

    四川省科技计划资助

    国土资源部放射性与稀有稀散矿产重点实验室开放课题

详细信息
  • 中图分类号: TF19 TQ073 TQ026

Test of Using Non Highly Purified Scandia Preparation of Highly Purified Anhydrous Scandium Trichloride Fused Salt

  • 采用惰性气体气流中一步快速升温脱除氯化铵和剩余结晶水工艺,利用非高纯氧化钪制备高纯无水氯化钪熔盐.工艺条件的影响试验结果表明:在脱氯化铵和剩余结晶水阶段温度为400℃、保温时间为120 min、升温速度为11℃/min、氯化铵与氧化钪重量比=1.8:1、氧化钪与辅盐重量比=1:5、惰性气体流量为6.0L/min的综合工艺条件下,高纯无水氯化钪熔盐中钪的水解率为1.95%.扫描电镜形貌及电子探针微区成分分析表明,高纯无水氯化钪熔盐结晶状态较好,其他杂质元素的含量较低.