某低品位铅锌矿选矿工艺研究

程倩, 王明, 万宏民, 宁新霞, 李洁. 某低品位铅锌矿选矿工艺研究[J]. 矿产综合利用, 2021, (1): 65-71. doi: 10.3969/j.issn.1000-6532.2021.01.010
引用本文: 程倩, 王明, 万宏民, 宁新霞, 李洁. 某低品位铅锌矿选矿工艺研究[J]. 矿产综合利用, 2021, (1): 65-71. doi: 10.3969/j.issn.1000-6532.2021.01.010
Cheng Qian, Wang Ming, Wan Hongmin, Ning Xinxia, Li Jie. Study on Mineral Processing Technology for a Low-grade Lead-zinc Ore[J]. Multipurpose Utilization of Mineral Resources, 2021, (1): 65-71. doi: 10.3969/j.issn.1000-6532.2021.01.010
Citation: Cheng Qian, Wang Ming, Wan Hongmin, Ning Xinxia, Li Jie. Study on Mineral Processing Technology for a Low-grade Lead-zinc Ore[J]. Multipurpose Utilization of Mineral Resources, 2021, (1): 65-71. doi: 10.3969/j.issn.1000-6532.2021.01.010

某低品位铅锌矿选矿工艺研究

详细信息
  • 中图分类号: TD952

Study on Mineral Processing Technology for a Low-grade Lead-zinc Ore

  • 某铅锌矿石类型为磁黄铁矿铅锌矿石和黄铁矿—磁铁矿铅锌矿石,其中金属矿物主要是闪锌矿、磁黄铁矿,其次是黄铁矿、磁铁矿、方铅矿等,脉石矿物为石英、方解石、长石、白云母等,矿石中铅、锌、硫品位分别是0.47%、2.77%、4.27%,硫化铅占总铅的89.52%,氧化铅占总铅的4.37%,硫化锌占总锌的97.04%,氧化锌占总锌的1.74%.采用"铅锌优先浮选—铅、锌粗精矿浮磁联合精选"工艺流程进行该矿石的选矿试验,结果表明,在磨矿细度为-0.074 mm 75%条件下,经1粗1扫3精选铅、1粗1扫3精选锌,浮选精矿再经磁选,获得铅品位50.82%、铅回收率62.59%、含银343.02 g/t的铅精矿;锌品位45.42%、锌回收率79.26%、含银12.73 g/t的锌精矿;磁性产品中铅品位1.38%、铅回收率4.19%、锌品位11.83%、锌回收率6.15%.